Author(s): Abubakr A; Soliman A;
Concrete protective structures are mainly meant to withstand impact loads. However, fire events weaken concrete and reduce its impact resistance. This study investigated the impact behaviour of steel-fibre-reinforced alkali-activated slag (AAS) concrete before and after exposure to elevated temperatures (i.e., 200 °C, 400 °C, and 600 °C). Hydration produc ...