| Keyword search (4,164 papers available) | ![]() |
"nickel-based superalloy" Keyword-tagged Publications:
| Title | Authors | PubMed ID | |
|---|---|---|---|
| 1 | Influence of Homogenization and Solution Treatments Time on the Microstructure and Hardness of Inconel 718 Fabricated by Laser Powder Bed Fusion Process. | Fayed EM, Shahriari D, Saadati M, Brailovski V, Jahazi M, Medraj M | 32516909 ENCS |